SCC Crack initiation in nickel based alloy welds in hydrogenated steam at 400°c

Fichier principal
Vignette du fichier
201600001374.pdf (3.83 Mo) Télécharger le fichier
Origine Fichiers produits par l'(les) auteur(s)
Licence

Dates et versions

hal-02442236 , version 1 (18-03-2020)

Licence

Identifiants

  • HAL Id : hal-02442236 , version 1

Citer

E. Chaumun, C. Guerre, J. Crepin, C. Duhamel, M. Sennour, et al.. SCC Crack initiation in nickel based alloy welds in hydrogenated steam at 400°c. International Cooperative Group on Environmentally-Assisted Cracking of Water Reactor Materials (ICG-EAC) annual meeting, Institute of Metal Research, Chinese Academy of Sciences (IMR, CAS), May 2016, Qindao, China. ⟨hal-02442236⟩