C. Guerre, J. Crepin, M. Sennour, C. Duhamel, E. Heripre, et al.. SCC crack initiation of alloy 82 in hydrogenated steam at 400 degrees c. Réunion annuelle de l'ICG EAC, May 2015, Ann Harbor, United States. ⟨cea-02500826⟩